Why do 3D printed parts need tolerances?
Parts shrink/expand, have layer error, and shift in finishing. CAD-exact fits can be too tight or too loose.
Tolerance
Practical clearance and fit guidance for assembled parts across print processes.
Parts shrink/expand, have layer error, and shift in finishing. CAD-exact fits can be too tight or too loose.
Many teams test ~0.2–0.4mm per side on FDM and ~0.1–0.25mm on SLA. Always validate with coupons for material and size.
Print a small mating sample before the full part to lock clearance and reduce scrap cost.
Real Output
Parts we printed in-house on FDM, SLA and DLP machines. See more in the print gallery.
Usually you need more clearance than machining. Ultra-tight fits may need finishing or another process.
Tell us the target fit and mating method — we can help pick process and design clearance.